GH3030 Chemical Composition




C
Si
Mn
P
S




≤0.12
≤0.8
≤0.7
≤0.03
≤0.02




Cr
Ni
Al
Ti
Fe




19-22
Rem
≤0.15
0.15-0.35
≤1.5




Product Mechanical Property




Yield Strength
Tensile Strength
Elongation






ó 0.2/MPa
ó b/MPa
δ5%






320
635
35






Product Physical Property
Density
8.4g/cm3
Melting Point
1374~1420℃
Magnetic Property
Non-magnetic
Product Thermal conductivity
θ/℃
100
200
300
400
500
600
700
800
900
λ/(W/(m·C))
15.1
16.3
18
19.3
20.9
22.2
23.4
25.1
26.4
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 details
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 supplier
Danyang Kaixin Alloy Materials Co., Ltd. was founded on April 18th, 2007, covering an area of 13500 square meters with a registered capital of 20 million yuan. It is a professional enterprise engaged in independent production,research and development of high performance alloy materials such as precision alloy, high temperature alloy, nickel-based special welding wire, corrosion resistant alloy and so on. It is Jiangsu Province private science and technology enterprise, small and medium-sized technology-based enterprise, employee entrepreneurship base, Zhenjiang Harmony Enterprise, 2017 Jiangsu Top 100 high-tech enterprises with the most growth and 2020 South Jiangsu National Gazelle enterprise in Independent Innovation Demonstration Zone. Our company will add the most advanced 3.5 tons vacuum melting furnace and 5 tons atmosphere protection electroslag furnace to expand 2 nickel-based welding wire production lines, improving the production capacity of the company greatly in 2023. At the same period, the expansion project with annual 2000 tons output of nickel-based welding materials has been started and will continue to increase R&D investment. Since 2020, our R&D investment has reached 10 million. At present, we have cooperated with Beijing Steel Research Institute Nak to establish the "National Steel Material Testing Center - Joint Laboratory" and cooperated with Jiangsu Provincial Science and Technology to establish Zhenjiang Microwave Communication materials Engineering Center and Jiangsu (Kaixin) Nickel-based Superalloy Engineering Technology Research Center. From 2022 to 2025, our company will gradually transform from civilian to military, from mass products to science and technology products, and gradually move to the ranks of "high, refined, sophisticated, specialized and special" production. To this end, we will combine the existing research and development, production, testing and etc advantages to continue to expand our research and development team, continuing to make progress from exploration and testing.
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 supplier
1、Accept customized products: Our existing 50kgs Vacuum induction furnace and 100kg electroslag remelting furnace can achieve new product development for our customers. 2、Attach great importance to site management, 6S has been successfully implemented for many years with high visualization degree and quality risk reduction; 3、We are the source factory with production and testing capabilities 4、We have passed ISO9001:2015 quality management system standard and our process is controllable 5、Our delivery time is controllable 6、Perfect after-sales service that each customer will have a special documentary personnel, who is responsible for communicating with customers, including delivery, quality, technology and other details.
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 supplier
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 factory
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 factory
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 manufacture
GH3030 GH30 XH78T Superalloys Wire Strip Rod Tube Plate Nimonic80A nickel alloy kovar invar 36 factory

1. Who are we?

Danyang Kaixin Alloy Materials Co., Ltd. is headquartered in Danyang, Jiangsu, China. It was established on April 18, 2007. It is an enterprise specializing in the independent production and research and development of high-performance alloy materials such as precision alloys, high-temperature alloys, and nickel-based welding wires.

2. What is your product range?

Mass production products (Inconel718, Inconel , GOST, GB/T standard materials. Most products have passed ROHS testing, and one of the Inconel625 welding wires has obtained ABS certification.

3. What are the advantages of price and quality?

We have our own production and inspection equipment. There are always pre-production samples before mass production, and there are always final inspections before shipment.

4. Do you provide samples?

Yes, we provide samples if needed, but customers need to pay the sample fee.

5. Can I visit your factory before ordering?

Of course, you are welcome to visit the factory.

Presenting the KX-Alloy line of high-performance superalloys, consisting of GH3030, GH30, XH78T, Superalloys Cord, Remove, Pole, Tube, Plate, Nimonic80A, nickel alloy Kovar, and Invar 36. These products are made from a mix of nickel, iron, and various other steels to produce a resilient and reputable item.

GH3030, GH30, XH78T, and Nimonic80A are all alloys that are nickel-based are highly immune to deterioration and oxidation. These alloys have the tendency to be used in high-temperature applications, such as aerospace and chemical processing, as a result of their heat is great resistance stamina. The KX-Alloy line provides these alloys in a variety of systems, consisting of cords, strips, poles, tubes, and layers, production them functional and simple making use in an option of applications.

Kovar is a nickel-iron-cobalt alloy exhibits reduced thermal growth, production it well fit for use in digital applications. The KX-Alloy line provides Kovar in a variety of styles, consisting of cords, strips, poles, and layers, enabling for flexibility in designs and manufacturing.

Invar 36 is an alloy is iron nickel displays reduced thermal growth at ambient temperature levels, production it useful in applications such as accuracy tools and optical devices. The KX-Alloy line provides Invar 36 in a variety of systems.

All the items in the KX-Alloy line satisfy stringent industry criteria for efficiency and quality, ensuring that they are reputable and consistent. The products are made utilizing processes that are advanced decrease issues and ensure uniform residential buildings throughout the item.

Whether you're looking for a material to stand up to heats, exhibit reduced thermal growth, or provide phenomenal deterioration resistance, the KX-Alloy line of superalloys has you protected. With a variety of styles to choose from, you can find the perfect material for your specific application. Trust KX-Alloy for high-grade, reputable superalloys that deliver the efficiency you need.


Get a Free Quote

Our representative will contact you soon.
Email
Mobile
Name
Company Name
Message
0/1000

If you have any suggestions, please contact us

Contact Us
IT SUPPORT BY product gh3030 gh30 xh78t superalloys wire strip rod tube plate nimonic80a nickel alloy kovar invar 36-1

Copyright © Danyang Kaixin Alloy Material Co., Ltd. All Rights Reserved  -  Privacy Policy  -  Blog