GH4033 Chemical Composition





C
Cr
Ni
Al
Ti
Fe





0.03~0.08
19.0~22.0
Rem
0.60~1.00
2.40~2.80
≤4





Mn
Si
P
S
B
Ce





≤0.35
≤0.65
≤0.015
≤0.007
≤0.01
≤0.01





Product Heat Treatment institution





The hot-rolled bar for rotating parts is 1080℃±10℃, air cooling +700℃±10℃, 16h, air cooling. The bar and cold drawing bar for ordinary bearing parts are 1080℃, 8h, air cooling +700℃ or 750℃, 16h, air cooling. annular blank and forged round plate at 1080℃,8h, air cooling +750℃, 16h, air cooling.
















Product Physical Property
Density
ρ=8.2g/cm
Greenhouse resistivity
Greenhouse resistivity
magnetic property
non-magnetic
Product Thermal conductivity









θ/℃
100
200
300
400
500
600
700
800
900









λ/(W/(m·C))
11.3
12.97
14.64
16.32
17.99
20.08
22.59
25.11
27.62









Product Coefficient of Linear Expansion









θ/℃
20~100
20~200
20~300
20~400
20~500
20~600
20~700
20~800
20~900









α/10-6C-1
11.56
12.3
13.17
13.79
14.52
15.07
15.62
16.3
17.15









Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 manufacture
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 manufacture
Danyang Kaixin Alloy Materials Co., Ltd. was founded on April 18th, 2007, covering an area of 13500 square meters with a registered capital of 20 million yuan. It is a professional enterprise engaged in independent production,research and development of high performance alloy materials such as precision alloy, high temperature alloy, nickel-based special welding wire, corrosion resistant alloy and so on. It is Jiangsu Province private science and technology enterprise, small and medium-sized technology-based enterprise, employee entrepreneurship base, Zhenjiang Harmony Enterprise, 2017 Jiangsu Top 100 high-tech enterprises with the most growth and 2020 South Jiangsu National Gazelle enterprise in Independent Innovation Demonstration Zone. Our company will add the most advanced 3.5 tons vacuum melting furnace and 5 tons atmosphere protection electroslag furnace to expand 2 nickel-based welding wire production lines, improving the production capacity of the company greatly in 2023. At the same period, the expansion project with annual 2000 tons output of nickel-based welding materials has been started and will continue to increase R&D investment. Since 2020, our R&D investment has reached 10 million. At present, we have cooperated with Beijing Steel Research Institute Nak to establish the "National Steel Material Testing Center - Joint Laboratory" and cooperated with Jiangsu Provincial Science and Technology to establish Zhenjiang Microwave Communication materials Engineering Center and Jiangsu (Kaixin) Nickel-based Superalloy Engineering Technology Research Center. From 2022 to 2025, our company will gradually transform from civilian to military, from mass products to science and technology products, and gradually move to the ranks of "high, refined, sophisticated, specialized and special" production. To this end, we will combine the existing research and development, production, testing and etc advantages to continue to expand our research and development team, continuing to make progress from exploration and testing.
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 supplier
1、Accept customized products: Our existing 50kgs Vacuum induction furnace and 100kg electroslag remelting furnace can achieve new product development for our customers. 2、Attach great importance to site management, 6S has been successfully implemented for many years with high visualization degree and quality risk reduction; 3、We are the source factory with production and testing capabilities 4、We have passed ISO9001:2015 quality management system standard and our process is controllable 5、Our delivery time is controllable 6、Perfect after-sales service that each customer will have a special documentary personnel, who is responsible for communicating with customers, including delivery, quality, technology and other details.
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 details
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 details
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 manufacture
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 factory
Pure Nickel Strip Rod Tube Plate nickel based superalloy hastelloy c276 c22 c200 UNS N10276 invar 36 manufacture

1. Who are we?

Danyang Kaixin Alloy Materials Co., Ltd. is headquartered in Danyang, Jiangsu, China. It was established on April 18, 2007. It is an enterprise specializing in the independent production and research and development of high-performance alloy materials such as precision alloys, high-temperature alloys, and nickel-based welding wires.

2. What is your product range?

Mass production products (Inconel718, Inconel , GOST, GB/T standard materials. Most products have passed ROHS testing, and one of the Inconel625 welding wires has obtained ABS certification.

3. What are the advantages of price and quality?

We have our own production and inspection equipment. There are always pre-production samples before mass production, and there are always final inspections before shipment.

4. Do you provide samples?

Yes, we provide samples if needed, but customers need to pay the sample fee.

5. Can I visit your factory before ordering?

Of course, you are welcome to visit the factory.


KX-Alloy


If you are getting a professional superalloy long lasting and nickel-based appeal no additional compared to Pure Nickel Strip Rod Tube Plate. This alloy is comprised of various pure nickel-based superalloys, along with various other aspects towards make an item premium and challenging along with wear-resistant.


The Pure Nickel Strip from KX-Alloy is fantastic for utilize within a range of uses, featuring production of chemical operation equipment, gas-turbine petrochemical handling, and aspects. In addition, it is relied on interior the aerospace business when it relates to higher power additionally towards fatigue and rust.


The Poles are created coming from the alloy specific exact very same are best for producing types complicated components. The superalloy comprehended nickel-based the power and sturdiness, that makes it best for made use of in building and development ventures. Its own residential or commercial homes permit it to become much less likely towards deform under tension, offering you along with peace of mind your particular duty should carry on for an opportunity lengthy the future.


The Tubes are crafted along with outstanding reliability, permitting their made use of in the make of warmth equivalent products and exchangers. The Pure Nickel Strip Rod Tube Plate can easily endure higher ailments and it is exceptionally immune towards rust, that helps make it the option best discovered in extreme environments.


The Layers are fit towards a variation broad of, including for example storage container cellular linings and sheet-metal construction, where its own higher resilience and stamina could be obtained in useful. The KX-Alloy's Pure Nickel Strip Rod Tube Plate can easily endure the harshest of ailments, and its own invar 36 structure gives excellent security dimensional excessive temperature levels.


Get a Free Quote

Our representative will contact you soon.
Email
Mobile
Name
Company Name
Message
0/1000

If you have any suggestions, please contact us

Contact Us
IT SUPPORT BY product pure nickel strip rod tube plate nickel based superalloy hastelloy c276 c22 c200 uns n10276 invar 36-1

Copyright © Danyang Kaixin Alloy Material Co., Ltd. All Rights Reserved  -  Privacy Policy  -  Blog